Laser Doppler Micro-electrophoresis is the technique used to measure zeta potential. An electric field is applied to a solution of molecules or a dispersion of particles, which will then move with a velocity related to their zeta potential. This velocity is measured using a laser interferometric technique. Static Light Scattering is used to determine the molecular weight of proteins and polymers.
Capabilities/Accessories
- Size measurement from 0.6 nm – 6000 nm
- Sample concentrations from 0.1 ppm to 40% w/v
- Disposable capillary cell for zeta potential measurements to completely eliminate cross contamination are available
Example/Application areas
![TEM image of TiO2 powder](https://pp-prod-admin.it.su.se/polopoly_fs/1.207825!/image/image.jpg_gen/derivatives/article_505/image.jpg)
![Particle size distribution of the TiO2 powder (shown above on the TEM image) obtained by dynamic light scattering](https://pp-prod-admin.it.su.se/polopoly_fs/1.207826!/image/image.jpg_gen/derivatives/article_505/image.jpg)
Publications:
Spray drying of TiO2 nanoparticles into redispersible granules
Faure, B; Lindelov, JS; Wahlberg, M; Adkins, N; Jackson, P; Bergstrom, L
2010 | POWDER TECHNOLOGY | 203 (384-388)
Colloidal aspects relating to direct incorporation of TiO2 nanoparticles into mesoporous spheres by an aerosol-assisted process.
Petr O Vasiliev; Bertrand Faure; Jovice Boon Sing Ng; Lennart Bergstrom
2008 | Journal of Colloid and Interface Science | 319 (144-151)
Recharge Rates
MMK users: 80 SEK
With operator: additional 250 SEK/hour
Outside academic users: 160 SEK
With operator: additional 800 SEK/hour
Non-academic users: 320 SEK
With operator: additional 1000 SEK/hour